Contact Person : Helen Young
Phone Number : +86 189 3070 0197
WhatsApp : +8618930700197

Superalloy powder

Place of Origin MADE IN CHINA
Brand Name DATOP
Model Number GH4169
Minimum Order Quantity 5kgs
Price 5-5000usd
Packaging Details pvc bags, parcel, wooden box
Delivery Time 7-10 days
Payment Terms T/T, MoneyGram, Western Union
Supply Ability 5000kgs/day
Product Details
Material Supper Alloy Powder Shape Spherical
Application 3D Printing,powder Metallurgy
Leave a Message
Product Description

Superalloy powder

It refers to a class of metal materials based on iron, nickel and cobalt, which can work for a long time at a high temperature above 600 ° C and a certain stress environment. It is mainly used in high-performance engines. In modern advanced aero-engines, the use of superalloy materials accounts for 40% to 60% of the total engine mass, and is also widely used in nuclear power, chemical industry and other fields.

Grade Chemical composition Product Standard Particle size distribution
Major element Incidental element National standard American-Standard

 

 

 

625

(GH3625)

 

Cr:20.0-23.0

Mo:8.0-10.0

Nb:3.15-4.15

Fe:≤5.0

Si:≤0.50

Ni:Bal

 

Ti:≤0.40

Al:≤0.40

C:≤0.10

Co:≤1.00

S:≤0.015

P:≤0.015

O:≤0.01

 

 

 

GB/T

14992-2005

 

 

 

15-45μm

15-53μm

53-120μm

53-150μm

 

 

 

 

718

(GH4169)

 

Ni:50.0-55.0

Cr:17.0-21.0

Nb:4.75-5.25

Mo:2.80-3.30

Ti:0.65-1.15

Al:0.20-0.80

Cu:≤0.30

Fe:Bal

 

 

 

 

 

O:≤0.01

 

 

 

 

GB/T

14992-2005

 

 

 

 

15-45μm

15-53μm

53-120μm

53-150μm

 

 

 

713C

(K418)

 

Cr:11.5-13.5

Mo:3.8-4.8

Al:5.5-6.4

Ti:0.5-1.0

Nb:1.8-2.5

Ni:Bal

 

 

C:0.08-0.16

Fe:≤1.0

O:≤0.01

 

 

 

 

 

GB/T

14992-2005

 

 

 

15-45μm

15-53μm

53-120μm

53-150μm

 

 

 

 

 

939

 

Cr:21.5-23.5

Co:18-20

W:1.8-2.2

Nb:0.8-1.2

Ta:1.2-1.6

Ti:3.5-3.9

Al:1.7-2.1

Zr:0.05-0.14

Ni:Bal

 

 

 

 

C:0.13-0.18

B:0.004-0.015

O:≤0.003

 

 

 

 

 

 

GB/T

14992-2005

 

 

 

 

 

15-45μm

15-53μm

53-120μm

53-150μm

 

 

 

 

K4648

 

Cr:32.0-35.0

W:4.3-5.5

Mo:2.3-3.5

Al:0.7-1.3

Nb:0.7-1.3

Fe:≤0.5

C:0.03-0.1

 

B:≤0.008

Ce:≤0.030

Si:≤0.30

S:≤0.01

Y:≤0.04

Ca:≤0.02

O:≤0.02

 

 

 

GB/T

14992-2005

 

 

 

15-45μm

15-53μm

53-120μm

53-150μm O:≤0.01